Our diamond suspension is characterized by an accurate particle size
distribution of the diamond powder used and a high standard of quality.

Special attention is paid to an evenly spread and free of agglomerate
particle distribution. Due to the special viscosity the diamonds will hang in
poise for about 24 hours. Due to the viscosity-density ratio the diamonds will descent to the bottom when not being used for a longer time. The manufacturing process of the suspension and a specific conditioning of the diamonds used, guarantee that no agglomeration will occur in or after the process of sedimentation. After shaking the suspension a bit it will be again ready for use having evenly spread the contained diamonds.


Our diamond suspension is available from 0–0.25 micron up to 50 micron (other sizes on request) and can be either produced in:


  1. water-soluble formulation (W)

  2. oil-soluble formulation (O)

  3. and in one of the following viscosity: liquid, light paste-like, paste-like

With regard to viscosity and concentration the suspension can also be produced as per your specifications.